Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.495 kN/m | 2.82 pli | BS EN ISO 8067 1995 |
Zotefoams Plastazote® LD24 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |