Tear Strength 0.250 kN/m
1.43 pli
Split Tear Strength, ASTM D3574-F
Covestro Bayfill® 310 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Tear Strength 0.250 kN/m
1.43 pli
ASTM D 624
Eurofoam Porocell POR 300/60 Ethylene Octane Metallocene EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.