Mechanical Properties Metric English Comments
Tear Strength >= 0.0400 kN/m
>= 0.228 pli
P & P Technology Polyester Polyurethane Foam
Description- High performance acoustic and dust filtration foam with a density of 60 Kg/cubic meter with excellent fire resistance properties. Used in heating, ventilation, electronic, aeronautic, a..
Tear Strength 0.0400 - 10.5 kN/m
0.228 - 60.0 pli
Average value: 1.08 kN/m Grade Count:71
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..