Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0465 GPa @Temperature 649 °C, Time 360000 sec |
6.74 ksi @Temperature 1200 °F, Time 100 hour |
Stress Rupture Strength |
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |