Polymer Property : Modulus of Rupture = 3.48 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0240 GPa

@Temperature 816 °C
3.48 ksi

@Temperature 1500 °F
Pyrotek Pyrocast SCM-2600 High Wear Impact Refractory Castable
Pyrocast SCM-2600 is suited for use in aluminum applications where severe wear is a factor. It is a high purity silicon carbide based refractory with low cement content.ApplicationsHigh erosion are..
Modulus of Rupture 0.0240 GPa

@Temperature 1400 °C
3.48 ksi

@Temperature 2550 °F
Cold
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0240 GPa

@Temperature 110 °C
3.48 ksi

@Temperature 230 °F
Cold
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0240 GPa

@Temperature 110 °C
3.48 ksi

@Temperature 230 °F
Cold
Sharadaa Ceramics VELECRETE RC 108 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..
Modulus of Rupture 0.0240 GPa

@Temperature 1400 °C
3.48 ksi

@Temperature 2550 °F
Cold
Sharadaa Ceramics VELECRETE RC 108 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..