Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.023544 GPa @Temperature 1000 °C, Time 10800 sec |
3.4148 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.023544 GPa @Temperature 1400 °C, Time 10800 sec |
3.4148 ksi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories SFC-90SC High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.023544 GPa @Temperature 1000 °C, Time 10800 sec |
3.4148 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SFC-90W High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |