Polymer Property : Modulus of Rupture = 2.846 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.01962 GPa

@Temperature 1500 °C,
Time 10800 sec
2.846 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories CTC-65SH Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.01962 GPa

@Temperature 1000 °C,
Time 10800 sec
2.846 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.01962 GPa

@Temperature 110 °C,
Time 86400 sec
2.846 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.01962 GPa

@Temperature 110 °C,
Time 86400 sec
2.846 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.01962 GPa

@Temperature 110 °C,
Time 86400 sec
2.846 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.01962 GPa

@Temperature 1500 °C,
Time 10800 sec
2.846 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories MMCT-75 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.01962 GPa

@Temperature 1400 °C
2.846 ksi

@Temperature 2550 °F
Chosun Refractories SB50 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.01962 GPa

@Temperature 250 °C
2.846 ksi

@Temperature 482 °F
Chosun Refractories SB75 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.01962 GPa

@Temperature 1000 °C,
Time 10800 sec
2.846 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SFC-70 SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).