Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0193 GPa @Temperature 23.0 °C |
2.80 ksi @Temperature 73.4 °F |
|
Zircar Ceramics DAHP Dense Alumina Hearth Plate ZIRCAR Dense Alumina Hearth Plates are used for supporting loads in high temperature furnaces and other thermal process systems. These dense plates are made of fully sintered fine grain high purity .. |