Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.01619 GPa @Temperature 1350 °C, Time 10800 sec |
2.348 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PCT-AM-1 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |