Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00950 GPa @Temperature 954 °C |
1.38 ksi @Temperature 1750 °F |
|
Pyrotek Pyrocast ALFS Abrasion-Resistant Refractory Castable Pyrocast ALFS refractory is a high flow, fused silica castable. At low water levels (6.5-7%), Pyrocast ALFS exhibits outstanding flow characteristics.ApplicationsAluminum melting equipment Aluminum.. |