Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00294 GPa @Temperature 1100 °C |
0.426 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFCAST C SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.00294 GPa @Temperature 1100 °C |
0.426 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFCAST K High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.00294 GPa @Temperature 1100 °C |
0.426 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.00294 GPa @Temperature 1100 °C |
0.426 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFINSUL 11 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00294 GPa @Temperature 1100 °C |
0.426 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00294 GPa @Temperature 1100 °C |
0.426 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00294 GPa @Temperature 1100 °C |
0.426 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00294 GPa @Temperature 1100 °C |
0.426 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFCAST C High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |