Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.363 GPa @Temperature 500 °C |
52.6 ksi @Temperature 932 °F |
|
Advanced Ceramics ACL 2087 Lithium Alumino-Silicate A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL) |