Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0014715 - 0.0034335 GPa @Temperature 500 °C, Time 10800 sec |
0.21343 - 0.49799 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-110N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0024525 GPa @Temperature 1000 °C, Time 10800 sec |
0.21343 - 0.35571 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories INCT-110S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0034335 GPa @Temperature 500 °C, Time 10800 sec |
0.21343 - 0.49799 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0034335 GPa @Temperature 1000 °C, Time 10800 sec |
0.21343 - 0.49799 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories INCT-120S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0034335 GPa @Temperature 500 °C, Time 10800 sec |
0.21343 - 0.49799 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0044145 GPa @Temperature 1000 °C, Time 10800 sec |
0.21343 - 0.64028 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories INCT135S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0044145 GPa @Temperature 500 °C, Time 10800 sec |
0.21343 - 0.64028 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0044145 GPa @Temperature 1000 °C, Time 10800 sec |
0.21343 - 0.64028 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0044145 GPa @Temperature 1000 °C, Time 10800 sec |
0.21343 - 0.64028 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0014715 - 0.0044145 GPa @Temperature 1350 °C, Time 10800 sec |
0.21343 - 0.64028 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories INCT-170 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |