Modulus of Rupture 0.044145 GPa

@Temperature 250 °C
6.4028 ksi

@Temperature 482 °F
Chosun Refractories SBSN Bricks, Reaction Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.044145 GPa

@Temperature 1400 °C
6.4028 ksi

@Temperature 2550 °F
Chosun Refractories SBSN Bricks, Reaction Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).