Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.026487 GPa @Temperature 1500 °C, Time 10800 sec |
3.8417 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |