Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00830 GPa @Temperature 760 °C, Time 3.60e+6 sec |
1.20 ksi @Temperature 1400 °F, Time 1000 hour |
Stress Rupture Strength |
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |