Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00785 GPa @Temperature 110 °C |
1.14 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFCAST 80 High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.00785 GPa @Temperature 110 °C |
1.14 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFINSUL 7 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |