Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00480 GPa @Temperature 1538 °C |
0.696 ksi @Temperature 2800 °F |
|
Pyrotek Valcor® G Pre-Cast Shapes ApplicationsBurner blocks Skimmer blocks Cover blocks Specialty blocks Plungers Stirrers Spouts Feeder tubes AdvantagesProven performance in molten glass contact applications Smooth surface finish d.. |
|||
Modulus of Rupture | 0.00480 GPa @Temperature 1371 °C |
0.696 ksi @Temperature 2500 °F |
ASTM C268 |
BNZ Materials Blazecrete 2500 HS Dense Castable Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li.. |