Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00300 GPa @Temperature 110 °C |
0.435 ksi @Temperature 230 °F |
|
Pyrotek Pyrocast 80 Lightweight Castable Refractory Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to.. |