Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 0.000900 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000900 GPa

@Temperature 104 °C
0.131 ksi

@Temperature 219 °F
Dried; ASTM C268
BNZ Materials Bazelite 2300 Insulating Castable
Blaz 2300 is a lightweight, general purpose insulating castable. Can be used for back-up or exposed to furnace conditions. Used for one-shot linings, petrochemical heaters, combustion chambers and f..
Modulus of Rupture 0.000900 GPa

@Temperature 104 °C
0.131 ksi

@Temperature 219 °F
Dried; ASTM C268
BNZ Materials Bazelite 2300 LI Insulating Castable
Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u..
Modulus of Rupture 0.000900 GPa

@Temperature 1095 °C
0.131 ksi

@Temperature 2003 °F
ASTM C268
BNZ Materials Bazelite 2100 Insulating Castable
Blaz 2100 is a general purpose lightweight castable for use as an exposed hot face refractory or as a very thermally efficient back-up to a dense refractory lining. Can be installed by casting, gunn..
Copyright © lookpolymers.com All Rights Reserved