Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 9.62361e-8 - 0.0004905 GPa @Temperature 110 °C, Time 86400 sec |
0.0000139581 - 0.07114 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories INCT-50S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0002943 - 0.0004905 GPa @Temperature 1000 °C, Time 10800 sec |
0.04269 - 0.07114 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories MIX-3 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |