Modulus of Rupture 0.0004905 - 0.0014715 GPa

@Temperature 500 °C,
Time 10800 sec
0.07114 - 0.21343 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-100S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.0014715 GPa

@Temperature 500 °C,
Time 10800 sec
0.07114 - 0.21343 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-110S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.0014715 GPa

@Temperature 1000 °C,
Time 10800 sec
0.07114 - 0.21343 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories INCT-120N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.0024525 GPa

@Temperature 500 °C,
Time 10800 sec
0.07114 - 0.35571 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-120S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.0024525 GPa

@Temperature 1000 °C,
Time 10800 sec
0.07114 - 0.35571 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories INCT-135N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.0024525 GPa

@Temperature 500 °C,
Time 10800 sec
0.07114 - 0.35571 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT135S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.000981 GPa

@Temperature 500 °C,
Time 10800 sec
0.07114 - 0.142 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-50S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.000981 GPa

@Temperature 500 °C,
Time 10800 sec
0.07114 - 0.142 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-80N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.000981 GPa

@Temperature 1000 °C,
Time 10800 sec
0.07114 - 0.142 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories MIX-2 Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).