Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ultimate Bearing Strength | 3110 MPa | 451000 psi | e/D = 1.5 |
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |