Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ultimate Bearing Strength | >= 1807 MPa | >= 262100 psi | e/D = 2.0 |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4986 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4986.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |