Polymer Property : Bearing Yield Strength = 61900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Bearing Yield Strength 427 MPa
61900 psi
B-bar, 4 pt bend
Ceramic Process Systems AlSiC-10, 54 vol% SiC
Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone..