Polymer Property : Bearing Yield Strength = 476.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Bearing Yield Strength 476.4 MPa
69100 psi
Pin Type (e/D = 2.0)
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy
This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%..