Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bearing Yield Strength | 0.000262 MPa | 0.0380 psi | |
Pacific Sintered Materials FC-203-N Copper Iron Powdered Metal Applications:Excellent for self-lubricating parts and heavy duty bearingsEquivalent MPIF Specification: FC-1000-20All information provided by Pacific Sintered Metals. |