Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Torsional Stiffness | 472 MPa | 68500 psi | -20°C; ASTM D1043 |
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |