Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Torsional Stiffness | 1.38 - 127 MPa | 200 - 18500 psi | Average value: 14.2 MPa Grade Count:20 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |