Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 90.0 J @Temperature -30.0 °C |
66.4 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BC 40 SR2 000000 Nylon 6 PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified |
|||
Puncture Energy | 90.0 J @Temperature -30.0 °C |
66.4 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BC 40 SR2 000000 Nylon 6 PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified |