Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 40.0 - 71.0 J | 29.5 - 52.4 ft-lb | Average value: 49.1 J Grade Count:12 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |