Polymer Property : Puncture Energy = 58.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 58.0 J

@Temperature -30.0 °C
42.8 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makroblend® DP UT6000 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedinjection molding grade Makroblend DP UT6000* offers an exceptional low-temperature impact strength, good flowability and excellent chemical resis..
Puncture Energy 58.0 J

@Temperature -30.0 °C
42.8 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c..
Puncture Energy 58.0 J

@Temperature -30.0 °C
42.8 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch..
Puncture Energy 58.0 J

@Temperature -30.0 °C
42.8 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and..