Polymer Property : Puncture Energy = 52.4 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 71.0 J
52.4 ft-lb
Puncture Resistance @ max load, 23°C; ISO 6603-2
Eastman DuraStar DS2000 Polymer, Natural
Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver..
Puncture Energy 71.0 J
52.4 ft-lb
Puncture Resistance @ max load, 23°C; ISO 6603-2
Eastman DuraStar DS2110UVI Polymer, Natural
Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li..
Puncture Energy 71.0 J
52.4 ft-lb
Puncture Resistance @ max load, 23°C; ISO 6603-2
Eastman DuraStar MN621 Polymer, Natural
Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo..
Puncture Energy 71.0 J
52.4 ft-lb
Puncture Resistance @ max load, 23°C; ISO 6603-2
Eastman Eastar BR203 Copolyester
Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie..