Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® B 31 SK 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® B 31 SK 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S |
|||
Puncture Energy | 70.0 J | 51.6 ft-lb | Puncture Resistance @ max load, -10°C; ISO 6603-2 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 1804 Polycarbonate MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh.. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 3103 MAS157 Polycarbonate ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte.. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 3107 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minGeneral purposeHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpare.. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 3156 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru.. |
|||
Puncture Energy | 70.0 J | 51.6 ft-lb | Puncture energy -30°C |
Covestro Makrolon® 3158 Polycarbonate Key Features:Release agentUnfilledSuitable processing methods:Injection moldingExtrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated.. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® DP1-1821* Polycarbonate Developmental productMVR (300 °C/1.2 kg) 6.0 cm3/10 minHigh viscosityUV stabilizedEasy releaseInjection moldingAvailable in colorless transparent onlyPreprocessingMax. Water content |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® LTG3123 Polycarbonate PreprocessingMax. Water content |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® Rx1805 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® Rx2430 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 an.. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® LQ3187 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable i.. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® Rx2530 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 .. |
|||
Puncture Energy | 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® KU1-1230* Polycarbonate ISO 7391-PC,EFL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 8.5 cm3/10 minFlame retardant16 mm Triple wall sheet/B1 classification (DIN 4102)Medium viscosityUV stabilizedExtrusionAs of 1 Sept.. |