Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 8.09 J | 5.97 ft-lb | Dow Method |
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP) AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In.. |