Polymer Property : Puncture Energy = 47.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 47.0 J

@Temperature -40.0 °C
34.7 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Eastman Drystar 0827 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Puncture Energy 47.0 J
34.7 ft-lb
Puncture Resistance @Max Load, -30°C; ASTM D3763
Eastman Spectar® 14471 Copolyester
Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use ..
Puncture Energy 47.0 J
34.7 ft-lb
ISO 6603-2
Covestro Makroblend® DP UT6000 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedinjection molding grade Makroblend DP UT6000* offers an exceptional low-temperature impact strength, good flowability and excellent chemical resis..
Puncture Energy 47.0 J
34.7 ft-lb
ISO 6603-2
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c..
Puncture Energy 47.0 J
34.7 ft-lb
ISO 6603-2
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch..
Puncture Energy 47.0 J
34.7 ft-lb
ISO 6603-2
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and..