Mechanical Properties Metric English Comments
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
Eastman Eastar EB062 Copolyester
Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Eastar EB062 Copolyester
Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
Eastman Eastar MB002 Copolyester
Eastar copolyester MB002 is a resin specifically developed for extrusion blow molding containers in medical applications where aesthetics such as high clarity and gloss, coupled with high toughness ..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Eastar MB002 Copolyester
Eastar copolyester MB002 is a resin specifically developed for extrusion blow molding containers in medical applications where aesthetics such as high clarity and gloss, coupled with high toughness ..
Puncture Energy 41.0 J

@Temperature -40.0 °C
30.2 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Eastman Provista MP001 Copolymer
Provista Copolymer MP001 is a resin specifically developed for extrusion into profiles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
Eastman Provista MP002 Copolymer
Provista Copolymer MP002 is a resin specifically developed for extrusion into profiles for medical applications where aesthetics such as high clarity and gloss, coupled with design flexibility and e..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Provista MP002 Copolymer
Provista Copolymer MP002 is a resin specifically developed for extrusion into profiles for medical applications where aesthetics such as high clarity and gloss, coupled with design flexibility and e..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
Eastman Provista ST Copolymer
Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation m..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Provista ST Copolymer
Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation m..
Puncture Energy 41.0 J

@Temperature -40.0 °C
30.2 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Eastman Provista UVI Copolymer
Provista UVI is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh..
Puncture Energy 41.0 J

@Temperature -40.0 °C
30.2 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Eastman Provista UVO Copolymer
Provista UVO is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
Eastman Eastar GN078 Copolyester, Natural
Eastar Copolyester GN078 builds on the strength of Eastar Copolyester GN077 by offering improved melt strength and toughness. Eastar Copolyester GN078 does not meet FDA compliance but is an excellen..
Puncture Energy 41.0 J
30.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Eastar GN078 Copolyester, Natural
Eastar Copolyester GN078 builds on the strength of Eastar Copolyester GN077 by offering improved melt strength and toughness. Eastar Copolyester GN078 does not meet FDA compliance but is an excellen..