Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 2.80 - 2.80 J @Temperature -30.0 - -30.0 °C |
2.07 - 2.07 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 2.80 J Grade Count:1 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Puncture Energy | 2.80 J | 2.07 ft-lb | ISO 6603-2 |
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 2.80 J @Temperature -30.0 °C |
2.07 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 2.80 J @Temperature -30.0 °C |
2.07 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 2.80 J @Temperature -30.0 °C |
2.07 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 2.80 J @Temperature -30.0 °C |
2.07 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 2.80 J @Temperature -30.0 °C |
2.07 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow) |
|||
Puncture Energy | 2.80 J @Temperature -30.0 °C |
2.07 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow) |
|||
Puncture Energy | 2.80 J @Temperature -30.0 °C |
2.07 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance |
|||
Puncture Energy | 2.80 J @Temperature -30.0 °C |
2.07 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance |