Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 17.6 J | 13.0 ft-lb | 70°C High Speed Puncture Energy; ASTM D3763-97a |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |