Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 150 J | 111 ft-lb | ISO 6603-2 |
Lanxess Durethan® BC 40 SR2 000000 Nylon 6 PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified |