Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1346 J @Temperature -30.0 °C |
992.8 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® TP 036-052 000000 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, good flowability (Easy Flow), good heat-resistance |
|||
Puncture Energy | 1346 J @Temperature -30.0 °C |
992.8 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® TP 036-052 000000 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, good flowability (Easy Flow), good heat-resistance |