Mechanical Properties Metric English Comments
Puncture Energy 120 J
88.5 ft-lb
ISO 6603-2
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e..