Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.40 J | 1.03 ft-lb | ISO 6603-2 |
Lanxess Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6, 40% Glass Fiber + Mineral PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance |