Polymer Property : Puncture Energy = 1.29 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 1.75 J
1.29 ft-lb
Low Friction Puncture
NOVA Chemicals Surpass® FPs117-D Octene sLLDPE Film Resin  (discontinued **)
Applications: Lamination Film, coextruded sealant layer, high toughness filmInformation provided by Nova Chemicals