Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 0.859 J | 0.633 ft-lb | ExxonMobil Method |
ExxonMobil LD 071.LQ Blown Film Resin L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou.. |
|||
Puncture Energy | 0.859 J | 0.633 ft-lb | ExxonMobil Method |
ExxonMobil LD 071.LR Blown Film Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |