Polymer Property : Puncture Energy = 0.722 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 0.722 J
0.533 ft-lb
Low Friction Puncture
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin
Features: Excellent barrier propertiesHigh stiffnessGood processability Low gel Applications: Barrier filmsCo-extrusionDry food packagingInformation provided by Nova Chemicals
Puncture Energy 0.722 - 2.14 J
0.533 - 1.58 ft-lb
Average value: 1.36 J Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..