Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 0.791 J | 0.583 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 3404.48 Linear Low Density Polyethylene Resin Product Description: LL 3404.48 is a hexane medium density polyethylene cast film grade for applications requiring high strength and high stiffness. Films produced from this resin exhibit good tensi.. |
|||
Puncture Energy | 0.791 J | 0.583 ft-lb | ExxonMobil |
ExxonMobil LL 3404.48 Cast Film Resin
(discontinued **) LL 3404.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex.. |