Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 0.395 J | 0.292 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America.. |
|||
Puncture Energy | 0.395 J | 0.292 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene blown film grade for applications requiring high stiffness. It can also be used in cast films. Films produced from the resin e.. |