Charpy Impact, Unnotched 8.13 J
6.00 ft-lb
Pacific Sintered Materials F-241-S Iron Powdered Metal
Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-15All information provided by Pacific Sintered Metals.
Charpy Impact, Unnotched 8.13 J
6.00 ft-lb
Pacific Sintered Materials FCC-214-S High Carbon Copper Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI..
Charpy Impact, Unnotched 8.13 J
6.00 ft-lb
Pacific Sintered Materials FN-255-S(HT) Nickel Steel Powdered Metal
Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0208-130HTAll information provided by Pacific Sintered Metals.
Charpy Impact, Unnotched 8.13 J
6.00 ft-lb
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-214-S Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP..
Charpy Impact, Unnotched 8.13 J
6.00 ft-lb
PSM Industries Pacific Sintered Metals Iron F-241-S Powdered Metal
Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-15Information Provided by Pacific Sintered Metals, a division of PSM Industries
Charpy Impact, Unnotched 8.13 J
6.00 ft-lb
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S(HT) Powdered Metal
Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0208-130HTInformation Provided by Pacific Sintered Metals, a division of PSM Industries