Polymer Property : Charpy Impact, Unnotched = 67.8 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 67.8 J
50.0 ft-lb
PSM Industries PolyAlloys MIM-17-4PH sintered Stainless Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Charpy Impact, Unnotched 67.8 J
50.0 ft-lb
PSM Industries PolyAlloys MIM-4605 sintered Low Alloy Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..